White Metal Alloys have low friction and wearing properties making them ideal for use in machinery were smooth and reliable operation is critical. They have strong inertness and extreme hardness applied in service severe conditions excellent strength and high operating temperatures. White Metals are a family of alloys that contain Tin, Antimony and Copper along with other elements like Lead & Arsenic. They are commonly used in large machinery applications such as turbines and generators. Babbitt Metal contains Tin, Antimony & Copper with smaller amounts of elements such as Lead & Zinc. Babbitt Metal is commonly used in high speed & heavy load bearing applications such as automotive engines and heavy machinery. The special grades of white metals are tabulated for their properties are as follows: -
Product Name |
Product Description |
ASTM B23 Grade 1 Babbitt Alloy |
Chemical Composition: Tin: 90-92%, Lead: .35% max, Antimony: 4.0-5.0%, Copper: 4.0-5.0% Tin Based Babbitt that is slightly softer than Grade 2 Babbitt. For applications requiring high speed but less pressure. |
Babbitt Alloy #1 |
Chemical Composition: Tin: 90-92%, Lead: .0004% max, Antimony: 4.0-5.0%, Copper: 4.0-5.0% A Special High Purity Lead Free Tin Based babbitt that can be used for bearings found in commercial ovens, material pumps and transport equipment used for handling food grade materials. |
ASTM B23 Grade 2 (GEN) Genuine Babbitt |
Chemical Composition: Tin: 88-90%, Lead: .35% max, Antimony: 4.7-8.0%, Copper: 3.0-4.0%. It is used for high speed and low-pressure applications. Ideal for repairing older airplane, automobile, boat, tin based Babbitt and not Lead as a Babbitt and steel liner. They are good for old connecting rods, crank pins, compressors, cutters, centrifugal pumps, dynamos, bus and diesel train engines and railway car axle bearings that used a mill gearing, elevators, arbors, trimmers, steam cylinders, steam pumps, band saws, swing saws, and tube mills that turn at high speed. |
ASTM B23 Grade 3 Babbitt Alloy |
Chemical Composition: Tin: 83-85%, Lead: .35% max, Antimony: 7.5-8.5%, Copper: 7.5-8.5%. Heavy Duty Tin Based Babbitt for High Speed, High Loads and High Shock applications. They are also used as general-purpose high-speed Babbitt for thin bearings of light running machinery with light to medium pressures such as compressors, electric motors, pumps and stationary engine parts. |
Engine Babbitt Alloy |
Chemical Composition: Tin: 85.5-87.5%, Lead: .25% max, Antimony: 6.5-7.5%, Copper: 6.5-7.6%. This Babbitt Alloy is used for Ford Engines. |
ASTM B23 Grade 4 Babbitt Alloy |
Chemical Composition: Tin: 80.5-82.5%, Lead: .25% max, Antimony: 12.0-14.0%, Copper: 5.0-6.0% Originally designed as a Thrust Washer Babbitt, this hardware grade Babbitt alloy is used for various non-critical low speed applications. It is customized to prepare it for specific applications requiring Grade # 4 Babbitt. |
ASTM B23 Grade 5 Babbitt Alloy |
Chemical Composition: Tin: 61.0-63.0%, Lead: 24.0-26.0%, Antimony: 9.5-10.5%, Copper: 2.5-3.5% Customized for specific applications requiring Grade # 5 Babbitt. |
ASTM B23 Grade 6 Babbitt Alloy |
Chemical Composition: Tin: 35-37%, Lead: 50-52%, Antimony: Copper: 0.5-1.5%. Customized for specific applications requiring Grade 6 Babbitt. |
ASTM B23 Grade 10 Babbitt Alloy |
Chemical Composition: Tin: 9.3-10.7%%, Lead: 78.0-83.0%, Antimony: 14.5-17.5%, Copper: .6% Customized for specific applications requiring Grade 10 Babbitt. |
ASTM B23 Grade 13 Babbitt Alloy |
Chemical Composition: Tin: 5.5-6.5%, Lead: 83-85%, Antimony: 9.5-10.5%, Copper: .5% Lead Based Babbitts Designed for Mill Anchor for Knife Blades. |
Babbitt Alloy Special Grade |
Chemical Composition: Sn: Balance, Sb: 7% - 8%, Cu: 3% - 4%, Ni: 0.2% - 0.3%, Cd: 1% - 1.5%. |